FRP Glossary
Technical terms that appear in data sheets, quotes, and conversations with manufacturers. Grouped by category so you can use this as a reference during supplier evaluations.
Isophthalic resin: standard polyester resin. Good for water and mild chemicals. Cheaper, lower chemical resistance than vinyl ester.
Vinyl ester: the most common resin for industrial FRP. Excellent resistance to acids, alkalis and oxidizers.
Epoxy: high mechanical and thermal strength. Used for high-pressure pipe, solvent environments, and aerospace.
Gelcoat: outer decorative and UV-protection layer. Not to be confused with the inner chemical barrier (which some manufacturers wrongly call "gelcoat").
Surface veil: thin glass C-veil or synthetic veil used in the chemical barrier layer to create a resin-rich surface.
Chopped strand mat (CSM): random chopped fiberglass, used to conform to complex shapes.
Roving: continuous fiber strands, used in filament winding and pultrusion.
Woven roving: woven fabric of roving. Higher structural strength than mat.
Hand lay-up: manual application of fiber and resin layers with a roller. Flexible but operator-dependent.
Filament winding: resin-impregnated filaments wound on a rotating mandrel. Best for cylindrical tanks and pipes.
RTM (Resin Transfer Molding): fibers in a closed mold with injected resin. Repeatable, good for small-to-medium parts.
Pultrusion: continuous process for structural profiles (gratings, angles, structural shapes).
Curing: chemical reaction that solidifies resin. Can be at ambient temperature or accelerated with heat.
Post-cure: additional heat treatment to complete cure, typically 60–80°C for several hours.
Delamination: separation between laminate layers. Primary cause of structural failure.
Porosity: air bubbles trapped in resin. Chemically weak points.
Dry spot: area where fiber was not fully impregnated with resin. Appears more opaque.
Blistering: bubbles that form on gelcoat or chemical barrier after time in service, due to osmosis or chemical attack.
Crazing: surface microcracks. Indicates fatigue or residual stress.
Fiber blooming: fibers exposed on the surface due to chemical or mechanical erosion. Equipment is near end of life.
Cure burn: discolored zone (brown) from excessive exotherm during curing.
Barcol hardness: surface hardness test with a Barcol durometer. Typical value for vinyl ester: 35–40.
Ultrasonic thickness: thickness measurement via ultrasonic. Standard for non-destructive laminate verification.
Hydrostatic test: fill equipment with water at 1.25× design pressure to verify tightness and strength.
Holiday test (spark test): electrical continuity detector for gelcoat/inner chemical barrier discontinuities.
Acetone extraction: test to detect incompletely-cured resin.
Tg (glass transition temperature): temperature where resin transitions from rigid to flexible. Defines upper thermal limit of the equipment.
ASME RTP-1: American code for design and fabrication of FRP equipment for non-pressure service (atmospheric tanks, chemical containers).
ASME Sec X: code for pressure-rated FRP equipment.
ASTM D2583: standard method for Barcol hardness testing.
ASTM C581: standard method for evaluating chemical resistance of FRP laminates.
ISO 9001: quality management system. Doesn't guarantee technical quality but documents the processes.
NOM-009-STPS / NOM-033-STPS: Mexican standards for work at heights and confined spaces (relevant for plant inspections).
If a supplier uses a term from this list and can't explain what it means in their specific equipment, that's a signal. Serious suppliers speak this vocabulary fluently.
Initial glossary. Expand with terms specific to your industry.