Common bad practices

When a supplier offers 2–5% less, they're usually cutting something you can't see at a glance. These are the most common shortcuts.

1. Resin substitution

Most common: they quote premium vinyl ester and build with a generic isophthalic. The data sheet looks identical; service life is cut in half.

2. Thinner laminate

Spec calls for 8 mm; they deliver 6.8 mm. The weight difference is imperceptible; the structural difference is significant.

Correct thickness

  • Ultrasonic-measured at 5+ points
  • Within ±5% of nominal
  • QC-signed thickness report

Thinned laminate

  • Measured only at thickest point
  • 10–15% under nominal at edges
  • No formal report, only "visual inspection"

3. Incomplete cure

Reducing cure time speeds production but leaves unreacted resin. Detected with a Barcol hardness test — which almost nobody asks for.

Draft. Add photos of real defects.

Posted on • by PITSA FRP